Material Notes:
Thermoplastic Elastomer (TPE)Characteristics: KOSYN KTR101 is linear block copolymer made by solution polymerization which polymerizes butadiene and styrene in organic solvent. It is thermoplastics free of vulcanization and has superior tensile strength and elasticity.Applications: Asphalt roofing, waterproof agent, modifier and adhesives.Additional Notes: Bound Styrene: 29%Volatile Matter: 0.5%; ASTM D1416This product is so sensitive to sunlight and humidity that it can be tarnished and caused deterioration of quality if exposed. It is recommended to store it in cool and shady area lest it should be exposed to direct sunlight. Do not expose to incompatible materials or contaminants.Data provided by Korea Kumho Petrochemical Co., Ltd.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ISO 2781
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
5 sec; ASTM D2240
Tensile Strength, Ultimate 80.0 MPa
11600 psi
ASTM D412
Elongation at Break 580 %
580 %
ASTM D412
Modulus of Elasticity 0.0260 GPa
3.77 ksi
ASTM D412
Users viewing this material also viewed the following: