Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 10.24 g/cc
0.3699 lb/in³
Thermal Properties Metric English Comments
Melting Point 103 - 117 °C
217 - 243 °F
Solidus 103 °C
217 °F
Liquidus 117 °C
243 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 53 %
53 %
Lead, Pb 42.5 %
42.5 %
Tin, Sn 4.5 %
4.5 %