Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy 41 Bismuth Solder Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 41 Bismuth Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.44 g/cc
0.341 lb/in³
Thermal Properties Metric English Comments
Melting Point 100 °C
212 °F
Eutectic
Solidus 100 °C
212 °F
Liquidus 100 °C
212 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 50 %
50 %
Lead, Pb 28 %
28 %
Tin, Sn 22 %
22 %
Users viewing this material also viewed the following: