Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 100 °C | 212 °F | |
Indium Corp. Indalloy 41 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 100 °C | 212 °F | |
AIM 35.7Sn/35.7Pb/28.6Bi Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |