Indium Corp. Indalloy 36 Bismuth Solder Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 36 Bismuth Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.64 g/cc
0.348 lb/in³
Thermal Properties Metric English Comments
Melting Point 87.0 - 93.0 °C
189 - 199 °F
Solidus 87.0 °C
189 °F
Liquidus 93.0 °C
199 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 51.4 %
51.4 %
Indium, In 2.0 %
2.0 %
Lead, Pb 31.4 %
31.4 %
Tin, Sn 15.2 %
15.2 %