Indium Corp. Indalloy® 183 Au-Ge Solder Alloy

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 183 Au-Ge Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eutectic die attach.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 14.67 g/cc
0.5300 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 185 MPa
26800 psi
Modulus of Elasticity 72.74 GPa
10550 ksi
Shear Strength 185 MPa
26800 psi
Shear Bond Holding Strength
Thermal Properties Metric English Comments
CTE, linear 13.0 µm/m-°C

@Temperature 20.0 °C
7.22 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 44.0 W/m-K

@Temperature 85.0 °C
305 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 356 °C
673 °F
Eutectic
Solidus 356 °C
673 °F
Liquidus 356 °C
673 °F
Component Elements Properties Metric English Comments
Germanium, Ge 12 %
12 %
Gold, Au 88 %
88 %
Users viewing this material also viewed the following: