Polymer Property : Shear Strength = 185 MPa
Polymer Property :
Shear Strength =
185 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Shear Strength
185
MPa
26800
psi
Shear Bond Holding Strength
Indium Corp. Indalloy® 183 Au-Ge Solder Alloy
Eutectic die attach.Information provided by the manufacturer, Indium Corporation.