Indium Corp. 16-2212 Flux Thinner

Category Fluid , Solvent
Manufacturer Indium Corporation of America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. 16-2212 Flux Thinner.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
#16-2212 flux thinner is a clear fluid for use with Wave Solder Flux Series #2212, to compensate for evaporation losses.Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 0.789 g/cc

@Temperature 25.0 °C
0.789 g/cc

@Temperature 77.0 °F
0.795 g/cc

@Temperature 15.5 °C
0.795 g/cc

@Temperature 59.9 °F
Solids Content 0.00 %
0.00 %
Thermal Properties Metric English Comments
Flash Point 12.2 °C
54.0 °F
TCC
Chemical Properties Metric English Comments
Acid Value 0.00
0.00