Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.795 g/cc @Temperature 15.5 °C |
0.795 g/cc @Temperature 59.9 °F |
|
Indium Corp. 16-2212 Flux Thinner #16-2212 flux thinner is a clear fluid for use with Wave Solder Flux Series #2212, to compensate for evaporation losses.Information provided by the manufacturer, Indium Corporation of America. |
|||
Specific Gravity | 0.795 g/cc @Temperature 25.0 °C |
0.795 g/cc @Temperature 77.0 °F |
|
Indium Corp. WF-9940 Wave Solder Flux WF-9940 is a highly active no-clean wave solder flux designed for use with through-hole and mixed-technology assemblies. It performs well with both Pb-free and Sn/Pb solders.WF-9940 is very heat st.. |