Indium Corp. 16-1081 Flux Thinner

Category Fluid , Solvent
Manufacturer Indium Corporation of America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. 16-1081 Flux Thinner.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
16-1081 flux thinner is for use with Wave Solder Flux 1081, to maintain specific gravity during use.Physical PropertiesColor: ClearInformation provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 0.806 g/cc

@Temperature 25.0 °C
0.806 g/cc

@Temperature 77.0 °F
0.812 g/cc

@Temperature 15.5 °C
0.812 g/cc

@Temperature 59.9 °F
Solids Content 0.00 %
0.00 %
Thermal Properties Metric English Comments
Flash Point 18.3 °C
65.0 °F