Polymer Property : Specific Gravity = 1.104 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.104 g/cc

@Temperature 25.0 °C
1.104 g/cc

@Temperature 77.0 °F
Indium Corp. #1210 Battery Flux
FeaturesWide process windowLow fumingMinimal residueMinimizes corrosion#1210 Battery Flux was specially formulated for high volume cast-on-strap manufacturing where rapid evaporation of solvent is n..