Hyosung Topilene J742 PP

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Hyosung Co.
Trade Name Topilene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hyosung Topilene J742 PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
J742 Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactHigh stiffnessInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 25 g/10 min
25 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 87
87
ASTM D785
Tensile Strength, Yield 29.4 MPa
4270 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Izod Impact, Unnotched 0.735 J/cm
1.38 ft-lb/in
ASTM D256
0.441 J/cm

@Temperature -10.0 °C
0.827 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648
Vicat Softening Point 150 °C
302 °F
ASTM D1525
Flammability, UL94 HB
HB