Material Notes:
Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by Shakespeare Company.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
Calculated from diameter of 0.28 mm and product yield of 14271 m/kg.
Fiber Count 700 dtex
630 denier
Per Filament
Mechanical Properties Metric English Comments
Elongation at Break 34 %
34 %
Tenacity 0.530 N/tex
6.00 g/denier
3.8 kg breaking load
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
Shrinkage 4.00 %

@Temperature 175 °C,
Time 601 sec
4.00 %

@Temperature 347 °F,
Time 0.167 hour
Electrical Properties Metric English Comments
Electrical Resistivity 10000 ohm-cm
10000 ohm-cm
Average
<= 15000 ohm-cm
<= 15000 ohm-cm