Huntsman Araldite GZ 7071 OX-65 Bisphenol A Epoxy Solution

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite GZ 7071 OX-65 Bisphenol A Epoxy Solution.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 455 to 525. Max color is 2.Comments/Applications: GT 7071 - 65% solids in Aromatic 100 (13%) and xylene (22%) High performance 2-package systems for coatings, flooring and general purpose. Viscosity, Gardner Holdt at 25°C: V-XData provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 900 - 1300 cP
900 - 1300 cP