Global GPC-105-S Enhanced Modulus, Structural Grade Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Global Polymers Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global GPC-105-S Enhanced Modulus, Structural Grade Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
ASTM D256