Huntsman Araldite GZ 540 X-90 Bisphenol A Epoxy Solution

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite GZ 540 X-90 Bisphenol A Epoxy Solution.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 233 to 278. Max color is 3.Comments/Applications: GY 6040 - 90% solids in xylene. General purpose bis A epoxy solution for use in 2-package maintenance and architectural coatings. Viscosity, Gardner Holdt at 25°C: Z4-Z6Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 6000 - 40000 cP
6000 - 40000 cP