Huntsman Araldite GT 6084 Bisphenol A Epoxy Solid Resin

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite GT 6084 Bisphenol A Epoxy Solid Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 875 to 1025. Max color is 1.Comments/Applications: Unmodified bis A "Type 4" epoxy. Specifically designed for esterification reactions to produce epoxy esters for high performance coatings.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 95.0 - 105 °C
203 - 221 °F
Softening Range