Hexcel® HexForce™ 384 Aramid Fabric

Category Other Engineering Material , Composite Fibers , Polymer , Thermoset , Aramid
Manufacturer Hexcel
Trade Name HexForce™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexForce™ 384 Aramid Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramids display excellent dimensional stability with a slightly negative coefficient of thermal expansion (-2.4 X 10-6/ºC.) They are resistant to chemicals with the exception of a few strong acids and alkalis.Aramids have excellent stability over a wide range of temperatures for prolonged periods. They show essentially no embrittlement or strength loss at temperatures as low as -320ºF (-196ºC). Aramids do not melt or support combustion but will start to carbonize at approximately 800ºF (427ºC).Information provided by Hexcel
Physical Properties Metric English Comments
Thickness 483 microns
19.0 mil
Fiber Count 1580 dtex
1420 denier
Warp yarn; Kevlar® 49
1580 dtex
1420 denier
Fill yarn; Kevlar® 49
Mechanical Properties Metric English Comments
Tensile Impact 694 J/cm
1300 ft-lb/in
Filling
726 J/cm
1360 ft-lb/in
Warp
Thermal Properties Metric English Comments
CTE, linear -2.40 µm/m-°C
-1.33 µin/in-°F
Maximum Service Temperature, Air 427 °C
801 °F
starts to carbonize
Minimum Service Temperature, Air -196 °C
-321 °F
Descriptive Properties Value Comments
Fabric Weight (oz/yd2) 10.7
Dry
Nominal Construction (count/in) 28
Warp
28
Fill
Weave Style 4x4 Basket
Users viewing this material also viewed the following: