Polymer Property : Thickness = 483 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 483 microns
19.0 mil
Polystrand ThermoPro™ IE7020X X-Ply Cross-Ply Polyethylene-Glass Composite
2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther..
Thickness 483 microns
19.0 mil
per ply, 8HS form
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, C2 Reinforced
Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel..
Thickness 483 microns
19.0 mil
Hexcel® HexForce™ 384 Aramid Fabric
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid..
Thickness 483 microns
19.0 mil
Overall; Arlon SQA-TMS-003
Arlon 51588R019 0.019" (0.483 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2, Layer 1: Cured Silicone RubberSide 2, Layer 2: Uncured Silicone Rubber Interleave: Polyethylene Appearanc..
Thickness 483 microns
19.0 mil
Substrate; Arlon SQA-TMS-003
Arlon 55572AA024 0.024" (0.610 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass This data represents typical values for the production material. The data should not be us..
Thickness 483 microns
19.0 mil
Substrate; Arlon SQA-TMS-003
Arlon 55578R030 0.0325" (0.825 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 1, Layer 2: Uncured Silicone Rubber Side 1, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Cured Silicone Rubber Appearance:..
Thickness 483 microns
19.0 mil
Substrate; Arlon SQA-TMS-003
Arlon 55578XA030 0.032" (0.813 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: 162 Style Fiberglass Side 1: Cured Silicone Rubber (Skim Coat)..
Thickness 483 microns
19.0 mil
Substrate; Arlon SQA-TMS-003
Arlon 55586XC028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material ..
Thickness 483 microns
19.0 mil
Substrate; Arlon SQA-TMS-003
Arlon 55866R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material ..
Thickness 483 microns
19.0 mil
Substrate; Arlon SQA-TMS-003
Arlon 55869R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia..
Thickness 483 microns
19.0 mil
Substrate; Arlon SQA-TMS-003
Arlon 55869R062 0.062" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia..
Thickness 483 microns
19.0 mil
Substrate; Arlon SQA-TMS-003
Arlon 55989R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia..
Thickness 483 microns
19.0 mil
Prime Coated 7500 Fiberglass, Substrate
Arlon R35121R063 0.063" (1.60 mm) Uncured Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured RubberSide 2: Uncured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material speci..
Thickness 483 microns
19.0 mil
Side 2; Arlon SQA-TMS-003
Arlon 51946C030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Wash Coat Appearance: Brown silicone rubber and gum on fiberglass..
Thickness 483 microns
19.0 mil
substrate; Arlon SQA-TMS-003
Arlon 55096R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 2523 fiberglass; Side 2: uncured silicone rubber
Thickness 483 microns
19.0 mil
Substrate; Arlon SQA-TMS-003
Arlon 55102R024 0.024" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material specifications.In..
Thickness 483 microns
19.0 mil
substrate; Arlon SQA-TMS-003
Arlon 55106R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber
Thickness 483 microns
19.0 mil
substrate; Arlon SQA-TMS-003
Arlon 55109R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass
Thickness 483 microns
19.0 mil
substrate; Arlon SQA-TMS-003
Arlon 55146R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber
Thickness 483 microns
19.0 mil
Style 162 Fiberglass, Substrate; Arlon SQA-TMS-003
Arlon 55146XA028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber This data represents typical values for the production mat..
Thickness 483 microns
19.0 mil
Substrate; Arlon SQA-TMS-003
Arlon 55149R028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red si..
Thickness 483 microns
19.0 mil
substrate; Arlon SQA-TMS-003
Arlon 55149R062 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass
Thickness 483 microns
19.0 mil
Aremco Pyro-Tape™ 682-PM High Temperature Tape Tri-layer silicone rubber/aluminum foil/ fiberglass with silicone adhesive
Applications Plasma Spray Masking Features Multi-ply construction replaces single-ply tapes permitting significant reduction in masking time. Shadow mask tape for HVOF (high velocity oxy- fuel) spr..
Thickness 483 microns
19.0 mil
substrate; Arlon SQA-TMS-003
Arlon 55279R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass
Thickness 483 microns
19.0 mil
Polystrand ThermoPro™ IE7021X ECR X-Ply Cross-Ply Polyethylene-Glass Composite
2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther..
Thickness 483 microns
19.0 mil
substrate; Arlon SQA-TMS-003
Arlon 55276R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber