H.C. Starck Grade D Titanium Carbonitride

Category Ceramic , Nitride
Manufacturer H.C. Starck
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Grade D Titanium Carbonitride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Narrow grain distribution and low oxygen contentHard metals (tooling and machining)CermetsBlack ceramics
Physical Properties Metric English Comments
Particle Size 1.0 - 1.5 µm
1.0 - 1.5 µm
Average
1.5 - 4.0 µm
1.5 - 4.0 µm
Laser Diffraction D50
Descriptive Properties Value Comments
TiC:TiN Ratio 50:50