H.C. Starck Grade A 01 Boron Nitride, BN

Category Ceramic , Nitride
Manufacturer H.C. Starck
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Grade A 01 Boron Nitride, BN.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
White powder.Solid lubricant for high-temperature applicationsMold release for die casting and injection moldingRaw material for cubic BNThermally conductive filler for polymersComposite ceramics, e.g. evaporation boatsStarting material for hot-pressed BN partsRefractories
Physical Properties Metric English Comments
Specific Surface Area 4.0 - 7.5 m²/g
4.0 - 7.5 m²/g
BET
Component Elements Properties Metric English Comments
B2O3 <= 0.15 %
<= 0.15 %