Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 4.0 m²/g | 4.0 m²/g | BET |
Nabaltec APYMAG® 40 Magnesium Hydroxide The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p.. |
|||
Specific Surface Area | 4.0 - 10 m²/g | 4.0 - 10 m²/g | BET |
Nabaltec NABALOX® NO 103 Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 4.0 - 7.0 m²/g | 4.0 - 7.0 m²/g | BET |
Nabaltec NABALOX® NO 615-30 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 4.0 - 7.0 m²/g | 4.0 - 7.0 m²/g | BET |
Nabaltec NABALOX® NO 625-30 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 4.0 m²/g | 4.0 m²/g | BET |
Nabaltec NABALOX® NO 645 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Specific Surface Area | 4.0 m²/g | 4.0 m²/g | |
Momentive Performance Materials AC-6028 Boron Nitride (BN) Powder Grade AC-6028 consists of agglomerated particles of hexagonal Boron Nitride (BN) with a mean particle size between 100 and 150µ. It exhibits the unique properties of BN in a form readily used in.. |
|||
Specific Surface Area | 4.0 - 7.5 m²/g | 4.0 - 7.5 m²/g | BET |
H.C. Starck Grade A 01 Boron Nitride, BN White powder.Solid lubricant for high-temperature applicationsMold release for die casting and injection moldingRaw material for cubic BNThermally conductive filler for polymersComposite ceramics, e.. |
|||
Specific Surface Area | 4.0 - 6.0 m²/g | 4.0 - 6.0 m²/g | BET |
H.C. Starck Grade B-hp Silicon Carbide, SiC High purity Beta SiC powder. Min. 99.995%.Sliding bearingsSeal ringsWear partsKiln furniture, crucibles, heating elements, burner nozzles, heat exchangersSemiconductor handling partsComponents for w.. |
|||
Specific Surface Area | 4.0 - 6.0 m²/g | 4.0 - 6.0 m²/g | BET |
H.C. Starck Grade UF 05 Silicon Carbide, SiC Alpha SiC for hot-pressing and infiltration.Sliding bearingsSeal ringsWear partsKiln furniture, crucibles, heating elements, burner nozzles, heat exchangersSemiconductor handling partsComponents for.. |
|||
Specific Surface Area | 4.0 - 6.5 m²/g | 4.0 - 6.5 m²/g | BET |
H.C. Starck Grade B 50 Boron Nitride, BN White powder.Solid lubricant for high-temperature applicationsMold release for die casting and injection moldingRaw material for cubic BNThermally conductive filler for polymersComposite ceramics, e.. |
|||
Specific Surface Area | 4.0 - 8.0 m²/g | 4.0 - 8.0 m²/g | BET |
H.C. Starck Grade C Aluminum Nitride AIN High thermally conductive ceramicsComposite ceramicsSiAlONsHeat sinksElectrically insulating packages for electronicsCrucibles for metals and salt meltsThermally conductive filler for polymersCompon.. |
|||
Specific Surface Area | 4.0 m²/g | 4.0 m²/g | |
Zircar Zirconia ZYBF-2 Zirconia Bulk Fiber Insulation Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed .. |
|||
Specific Surface Area | 4.0 - 8.0 m²/g | 4.0 - 8.0 m²/g | B.E.T. |
ATI Wah Chang Jet Milled Zirconium Oxide, ZrO2 Jet Milled. A fine, white powder.Information provided by ATI Wah ChangTypical Analysis: On Zr oxide basis |
|||
Specific Surface Area | 4.0 m²/g | 4.0 m²/g | ATO 40-45-0 (BET) |
Arkema Group ORGASOL® 2001 EXD Nat 1 Polyamide 12, Food Contact Approved Information provided by Arkema Group |
|||
Specific Surface Area | 4.0 m²/g | 4.0 m²/g | |
BASF Sicopal® Green K 9610 Color Additive Chemical Structure: Co/Ti/Ni/Zn-oxideApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA PETP, CA/CAB and UPRecommendations for food applicat.. |
|||
Specific Surface Area | 4.0 m²/g | 4.0 m²/g | |
BASF Sicopal® Brown K 2595 Color Additive Chemical Structure: Zn/Fe-oxideApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA PETP, CA/CAB and UPRecommendations for food applications: .. |
|||
Specific Surface Area | 4.0 m²/g | 4.0 m²/g | |
Zircar Zirconia ZYBF-2 Zirconia Bulk Fiber Insulation Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed .. |