H.C. Starck Amperit® 825.1 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3)

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer H.C. Starck
Trade Name Amperit®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 825.1 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Particle Size 15 µm
15 µm
Maximum of 5% less than
62 µm
62 µm
Minimum of 95% less than
88 µm
88 µm
100% less than
Component Elements Properties Metric English Comments
Al2O3 <= 0.60 %
<= 0.60 %
Fe2O3 <= 0.30 %
<= 0.30 %
Hafnium, Hf 0.20 - 2.5 %
0.20 - 2.5 %
SiO2 <= 0.60 %
<= 0.60 %
TiO2 >= 0.30 %
>= 0.30 %
Y2O3 6.0 - 8.0 %
6.0 - 8.0 %
ZrO2 87.7 - 93.8 %
87.7 - 93.8 %