Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

H.C. Starck Amperit® 547.059 Tungsten Carbide-Nickel 88-12 (WC-Ni)

Category Ceramic , Carbide
Manufacturer H.C. Starck
Trade Name Amperit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 547.059 Tungsten Carbide-Nickel 88-12 (WC-Ni).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 4.70 - 5.60 g/cc
0.170 - 0.202 lb/in³
ASTM B417
Particle Size 17 - 22 µm
17 - 22 µm
10%
30 - 38 µm
30 - 38 µm
50%
44 µm
44 µm
Minimum of 99% less than
53 - 63 µm
53 - 63 µm
90%
62 µm
62 µm
100% less than
Component Elements Properties Metric English Comments
Carbon, C 5.4 - 5.8 %
5.4 - 5.8 %
Iron, Fe <= 0.20 %
<= 0.20 %
Nickel, Ni 11 - 13 %
11 - 13 %
Tungsten, W 81 - 83.6 %
81 - 83.6 %
Users viewing this material also viewed the following: