Gwent Electronic Materials D2071120D1 Polymer Dielectric

Category Fluid , Polymer
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials D2071120D1 Polymer Dielectric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Blue colored screen printable polymer dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode. The formulation is designed for maximum flexibility. Screen Printing Equipment: semi-automatic, automaticScreen Types: stainless steel, polyester, mesh 150 to 250tpiSubstrate: Polyester, PVC, Polycarbonate, or Alumina.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 39 - 41 %

@Temperature 150 °C
39 - 41 %

@Temperature 302 °F
Viscosity 5000 - 6500 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
5000 - 6500 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C
68.0 °F
sealed container
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 130 °C
0.250 hour

@Temperature 266 °F
30.0 min

@Temperature 80.0 °C
0.500 hour

@Temperature 176 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 310
Using a 230 mesh stainless steel screen
Solvent Resistance Acetone
Attack
Acetone
Attack
DMF
Attack
DMF
Attack
MEK
Full Attack
MEK
Full Attack
THF
Attack
THF
Attack