Guarniflon TENFIL TF 400 Polytetrafluoroethylene Thread Sealant

Category Polymer , Thermoplastic , Adhesives, Sealants, and Coatings , Fluoropolymer , PTFE
Manufacturer Guarniflon
Trade Name TENFIL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Guarniflon TENFIL TF 400 Polytetrafluoroethylene Thread Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TENFIL TF400 is a PTFE-based thread sealant in water dispersion, which increases the tightness of the threaded parts and prevents leakage of water. The product is intended for the assembly of fittings and threaded joints of different kinds of pipes.UL 1356 approved for use with METHANE, BUTANE, PROPANE, NATURAL GAS (GPL).Information provided by Guarniflon®
Physical Properties Metric English Comments
Solids Content 50 - 55 %
50 - 55 %
pH 4.0 - 6.0
4.0 - 6.0
Brookfield Viscosity 11000 - 13000 cP
11000 - 13000 cP
Surface Tension 38 dynes/cm
38 dynes/cm
Thermal Properties Metric English Comments
Boiling Point 100 °C
212 °F
Clash Berg Stiffness Temperature 0.000 °C
32.0 °F
Processing Properties Metric English Comments
Dry Time 1.00 hour

@Temperature 20.0 °C
1.00 hour

@Temperature 68.0 °F
Drying Air Flow Rate 9000 l/min

@Temperature 80.0 °C,
Time 80.0 sec
318 ft³/min (CFM)

@Temperature 176 °F,
Time 0.0222 hour
9000 l/min

@Temperature 50.0 °C,
Time 120 sec
318 ft³/min (CFM)

@Temperature 122 °F,
Time 0.0333 hour
Shelf Life 12.0 Month

@Temperature 4.00 - 35.0 °C
12.0 Month

@Temperature 39.2 - 95.0 °F
Descriptive Properties Value Comments
Chemical Resistance Alcohol
Good
Aliphatic Solvents
Good
Aromatic Solvents
Moderate
Ester
Moderate
Glycols
Good
Grease
Good
Ketones
Moderate
Oils
Good
Color Blue