Material Notes:
Information provided by Goodfellow.
Thermal Properties Metric English Comments
Melting Point 1900 °C
3450 °F
Component Elements Properties Metric English Comments
Molybdenum, Mo 16 %
16 %
Titanium, Ti 84 %
84 %