Goodfellow Copper 70/Zirconium 30 Alloy

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer Goodfellow
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Copper 70/Zirconium 30 Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Goodfellow.
Thermal Properties Metric English Comments
Melting Point 1140 °C
2080 °F
Component Elements Properties Metric English Comments
Copper, Cu 70 %
70 %
Zirconium, Zr 30 %
30 %