Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Garlock BLUE-GARD® 3300 Compressed Aramid Fiber Gasketing, Neoprene Binder

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Garlock Rubber Technologies
Trade Name BLUE-GARD®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock BLUE-GARD® 3300 Compressed Aramid Fiber Gasketing, Neoprene Binder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aramid fiber, high-temperature fillers, and neoprene (CR) binder. Handles service conditions with refrigerants and various petroleum-based oils. Excellent SealabilityUnique blend of aramid fibers, fillers, and a neoprene rubber binder provides improved torque retention and lowered emissions levelsMedia: Water, Saturated Steam, Refrigerants, Oils, FuelsInformation provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0579 lb/in³
Permeability 0.080
0.080
Gas Permeability, cc/min; DIN 3535 Part 4
Mechanical Properties Metric English Comments
Tensile Strength 15.5 MPa
2250 psi
across grain; ASTM F152
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 371 °C
700 °F
204 °C

@Pressure 8.27 MPa
400 °F

@Pressure 1200 psi
Continuous
Minimum Service Temperature, Air -73.3 °C
-100 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 10.6 kV/mm

@Temperature 121 °C,
Time 10800 sec
>= 269 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.125 in. thickness; ASTM D149
>= 15.4 kV/mm

@Temperature 121 °C,
Time 10800 sec
>= 392 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.0625 in. thickness; ASTM D149
2.87 kV/mm

@Thickness 3.17 mm
73.0 kV/in

@Thickness 0.125 in
100% RH for 96 hours; ASTM D149
3.07 kV/mm

@Thickness 1.59 mm
78.0 kV/in

@Thickness 0.0625 in
100% RH for 96 hours; ASTM D149
Descriptive Properties Value Comments
Color Black
Compressibility, % 7-17
ASTM F36
Creep Relaxation, % 18
ASTM F38
Sealability ASTM F37B, ml/hr 0.2
ASTM Fuel A
1
Nitrogen