Dielectric Strength >= 10.6 kV/mm

@Temperature 121 °C,
Time 10800 sec
>= 269 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.125 in. thickness; ASTM D149
Garlock BLUE-GARD® 3300 Compressed Aramid Fiber Gasketing, Neoprene Binder
Aramid fiber, high-temperature fillers, and neoprene (CR) binder. Handles service conditions with refrigerants and various petroleum-based oils. Excellent SealabilityUnique blend of aramid fibers, f..