Features: Antistat, Nucleated. Product does not contain animal derived components. Phthalate-free.Applications: Injection MoldingInformation Provided by Flint Hills Resources
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM D785
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus, 1% Secant 1399 MPa
202900 psi
ASTM D790
Izod Impact, Notched 0.300 J/cm

@Temperature 23.0 °C
0.562 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact 6.00 J

@Temperature 23.0 °C
4.43 ft-lb

@Temperature 73.4 °F
ASTM D5420
Tangent Modulus 1484 MPa
215200 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 109 °C
228 °F
ASTM D648