Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fibre Glast 549 Kevlar® Fabric

Category Other Engineering Material , Composite Fibers , Polymer , Thermoset , Aramid
Manufacturer Fibre Glast Developments Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fibre Glast 549 Kevlar® Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This was one of the first high strength synthetic fibers to gain acceptance in the reinforced plastic industry. Unlike the previous synthetic reinforcing fibers, Kevlar® has a considerably higher tensil strength and modulus than fiberglass. Kevlar® is usually used for structures requiring good stiffness, high abrasion resistance, and light weight. Current applications include lightweight boat hulls such as kayaks and canoes, aircraft fuselage panels and pressure vessels. Kevlar® may be used with epoxy or vinyl ester resins.General Properties for Kevlar®/Carbon Hybrid: Excellent thermal & dimensional stability; Performs with no strength loss up to temperatures of 320°F for extended periods; Lighter in weight than E-Glass with higher specific strengths; Sensitive to direct exposure from UV light; however, demonstrates little or no change in a composite when it is indirectly exposed to UV light; Will not melt or support combustion, however, it will begin to caramelize at approximately 800°FGeneral Properties for Kevlar®/Carbon Hybrid: Excellent thermal & dimensional stability; Performs with no strength loss up to temperatures of 320°F for extended periods; Lighter in weight than E-Glass with higher specific strengths; Sensitive to direct exposure from UV light; however, demonstrates little or no change in a composite when it is indirectly exposed to UV light; Will not melt or support combustion, however, it will begin to caramelize at approximately 800°F
Physical Properties Metric English Comments
Thickness 305 microns
12.0 mil
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Extended periods
Descriptive Properties Value Comments
Weave Pattern 4-Harness Satin
Weight (oz/sq yd) 5
Yarn Description, Fill 1140 Denier Kevlar® 49
Yarn Description, Warp 1140 Denier Kevlar® 49
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved