Material Notes:
Shutters high modulus low curving
Physical Properties Metric English Comments
Density 1.51 - 1.55 g/cc
0.0546 - 0.0560 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Tensile Strength at Break 41.0 MPa
5950 psi
ISO R 527
Tensile Strength, Yield 44.0 MPa
6380 psi
Elongation at Break 120 %
120 %
ISO R 527
Izod Impact, Unnotched 0.400 - 0.800 J/cm

@Temperature 23.0 °C
0.749 - 1.50 ft-lb/in

@Temperature 73.4 °F
ISO R180
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 - 87.0 °C

@Load 5.00 kg
185 - 189 °F

@Load 11.0 lb
ISO R306