Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Unirex N 2

Category Fluid , Lubricant , Lithium Gellant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Unirex N 2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UNIREX N greases are premium-quality, lithium-complex products suitable for high-temperature service in rolling-element bearings. These versatile greases can be used in a wide range of industrial applications and are particularly recommended for electric-motor lubrication. Unirex N 2 in an NLGI No. 2 grade and is preferred in most cases for application by hand packing or by grease gun. UNIREX N 3 is an NLGI No. 3 grade often used for special applications such as sealed-for-life electric motor bearings, vertically mounted bearings, and higher-speed applications. UNIREX N greases are not intended to be used under extreme pressure conditions where extra anti-welding properties are required. UNIREX N 2 meets the requirements of Lubricating Grease DIN 51825 - K2N - 20 and ISO L-XBDGB 2. UNIREX N 3 meets the requirements of Lubricating Grease DIN 51825 - K3N - 20 and ISO L-XBDGB 3.Because of their outstanding oxidation stability and resistance to softening at high temperatures, UNIREX N greases may be used in many applications such as oven-conveyor bearings, dryer-roller bearings, rotary steam joints, kiln-car bearings, induced-draft fan bearings, and equipment adjacent to high radiant heat such as ovens, soaking pits, etc. UNIREX N 2 is an NLGI No. 2 grade and is preferred in most cases for application by hand-packing or by grease gun. UNIREX N 2 is recommended for the lubrication of electric motors. It is suitable for NEMA (National Electric Manufacturers Association) Insulation Class A, B, and F motors. UNIREX N 3 is an NLGI No. 3 grade and is used for special applications such as sealed-for-life bearings, vertically-mounted bearings, and higher-speed bearings. Most of the uses for UNIREX N involve manual methods of application. Although UNIREX N 2 is suitable for use in automatic centralized systems, equipment served by these systems would normally not require the long-life properties of UNIREX N, since one of the functions of automatic systems is to replenish the lubricant at relatively short time intervals. UNIREX N 3 should not be used in such systems. Regardless of the level of oxidation stability of a grease, an increase in temperature will affect the rate of oxidation and thermal deterioration. Consequently, more frequent relubrication is required at higher temperatures. For UNIREX N greases, it is recommended that relubrication intervals not exceed one week of continuous service at 175°C. As temperatures approach 190°C, relubrication intervals should be daily or every shift.  Relubrication intervals will, of course, vary widely with the type of service and should be based primarily on the recommendations of the motor manufacturer.
Physical Properties Metric English Comments
Viscosity Measurement 95
95
Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 115 cSt
115 cSt
ASTM D445
Mechanical Properties Metric English Comments
Penetration 25
25
Penetration Change after 100000 Strokes, mm/10; ASTM D217
280
280
Worked 60 strokes, mm/10; ASTM D217
Oil Separation 1.5 %
1.5 %
mass % @ 100°C / 30 hrs; ASTM D6184
Thermal Properties Metric English Comments
Dropping Point 230 °C
446 °F
ASTM D2265
Descriptive Properties Value Comments
Color green
Flow Pressure, DIN 51805, hPa 900
@ -20°C
Grease Life, DIN 51821 (FE-9), hours 448
@ 140°C
Rust Prevention, Distilled Water pass
ASTM D665A
Soap/Thickener Type lithium complex
Structure smooth, buttery
Water Washout, ASTM D1264, wt% 3.7
@ 79°C
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved