Thermal Properties Metric English Comments
Dropping Point 230 °C
446 °F
ASTM D2265
ExxonMobil Unirex N 2
UNIREX N greases are premium-quality, lithium-complex products suitable for high-temperature service in rolling-element bearings. These versatile greases can be used in a wide range of industrial ap..
Dropping Point 230 °C
446 °F
ASTM D2265
ExxonMobil Unirex N 3
UNIREX N greases are premium-quality, lithium-complex products suitable for high-temperature service in rolling-element bearings. These versatile greases can be used in a wide range of industrial ap..
Dropping Point 230 °C
446 °F
Dow Corning MOLYKOTE® AS-810 GREASE
Silicone grease with wide service temperature range for starter clutchInformation provided by Dow Corning
Dropping Point 230 °C
446 °F
ASTM D2265
ExxonMobil Unirex N 2
UNIREX N greases are premium-quality, lithium-complex products suitable for high-temperature service in rolling-element bearings. These versatile greases can be used in a wide range of industrial ap..
Dropping Point 230 °C
446 °F
ASTM D2265
ExxonMobil Unirex N 3
UNIREX N greases are premium-quality, lithium-complex products suitable for high-temperature service in rolling-element bearings. These versatile greases can be used in a wide range of industrial ap..
Dropping Point 230 °C
446 °F
ChevronTexaco Delo® Synthetic Grease SF
FeaturesChevron Delo Synthetic Grease SF is a high performance grease specifically engineered for trailer wheel-ends operating in all conditions, even under the most extreme high and low temperature..