ExxonMobil Thermrex Series V-32

Category Fluid , Quenchant
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Thermrex Series V-32.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and thermal stability, demulsibility, and nonferrous compatibility. The use of such ingredients results in quench oils that provide uniform steel hardness, long batch life, resistance to sludge formation, and minimum deformation. Thermrex D-10, R-21, and V-32 are mineral-oil blends carefully selected to approximate 100 SUS at 100°F. They yield consistent Relative Cooling Indices (RCI) of 95 to 160. Thermrex F-43 is a fast quench oil augmenting selected base stocks with additive technology to provide an RCI of 195. In addition, Thermrex R-21, V-32, F-43 are "gapped" to yield controlled distillation ranges from specific base stocks.The Thermrex Series oils are excellent media for rapidly cooling alloy steels to achieve optimum strength and toughness. The selection of the particular grade of quench oil depends on the cooling rate desired to prevent cracking and distortion. Thermrex Series oils D-10, R-21, V-32, and F-43 are most effective with agitation at batch temperatures of less than 150°F.
Physical Properties Metric English Comments
Specific Gravity 0.8618 g/cc
0.8618 g/cc
Kinematic Viscosity at 40°C (104°F) 16 cSt
16 cSt
Thermal Properties Metric English Comments
Pour Point -3.00 °C
26.6 °F
Flash Point 176 °C
349 °F
ASTM D92
Descriptive Properties Value Comments
Cooling Rate, ASTM D6200, F/Sec 116
GM Quenchometer, %Quench Time, sec 19
ASTM D3520
GM Quenchometer, Relative Cooling Index 148/162
ASTM D3520