Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 16 cSt
16 cSt
Base Oil; ASTM D445
Nye Lubricants 140C (SO) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 16 cSt
16 cSt
Base Oil; ASTM D445
Nye Lubricants 724L (RL) Rheolube Grease
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 16 cSt
16 cSt
Base Oil; ASTM D445
Nye Lubricants DHL-400 Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 16 cSt
16 cSt
ExxonMobil Thermrex Series V-32
The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and ..
Kinematic Viscosity at 40°C (104°F) 16 cSt
16 cSt
ExxonMobil Thermrex Series V-32
The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and ..