Material Notes:
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in thin wall applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.Key Features:Recommended for applications requiring excellent flex fatigue resistance.Recommended for applications requiring excellent ozone resistance.Designed for improved UV resistance.EU and China RoHS compliantApplications:Automotive- Seals, Gaskets and Weather SealsUses:Automotive Applications Automotive Exterior Trim Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 51

@Thickness 2.00 mm,
Time 15.0 sec
51

@Thickness 0.0787 in,
Time 0.00417 hour
ISO 868
Tensile Strength, Yield 11.3 MPa
1640 psi
Across Flow; ASTM D638
Elongation at Break 32 %
32 %
Across Flow; ASTM D638
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Descriptive Properties Value Comments
Change in Mass in IRM 903 Oil at 257°F for 70 hr 99
Color Black
Form Pellets