Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 2010 MPa | 292000 psi | 0.5 in/min; ASTM D790B |
ExxonMobil PP7905E1 Polypropylene Homopolymer Product Description: A high crystallinity, low impact strength copolymer resin designed for compounding base or injection molding applications requiring very high melt flow rate.Availability: North.. |
|||
Flexural Modulus, 1% Secant | 2010 MPa | 291000 psi | 0.5 in/min; ASTM D790B |
ExxonMobil PP1074KNE1 Polypropylene Homopolymer Product Description: A nucleated, medium flow rate homopolymer resin with mold release and anti-static properties. It is suitable for general purpose injection molding.Availability: North America .. |