ExxonMobil POLYBILT™ PB 152 Bitumen Modifier Resin  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil POLYBILT™ PB 152 Bitumen Modifier Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polybilt PB 152 is an 18% VA copolymer that yields modified bitumen blends with good storage stability, increased softening point, increased high temperature viscosity and decreased penetration. PB 152 can be blended using conventional equipment, Blending time will depend on the shear rate of the equipment used and temperature. The recommended temperature range is 330 to 350°F.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.941 g/cc
0.0340 lb/in³
ExxonMobil Method
Vinyl Acetate Content 19.3 %
19.3 %
ExxonMobil Method
Melt Flow 2.5 g/10 min
2.5 g/10 min
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 85.6 °C
186 °F
Peak Melting Temperature; ExxonMobil Method
Vicat Softening Point 61.7 °C
143 °F
ASTM D1525
Descriptive Properties Value Comments
Features Thermal Stabilizer
Users viewing this material also viewed the following: