Polymer Property : Vicat Softening Point = 143 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 61.7 °C
143 °F
ASTM D1525
ExxonMobil Escorene™ FL 00714 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00714 is an easy processable grade for extrusion coating, co-extrusion coating and cast film. This grade offers excellent heat sealing characteristics and excellent optical p..
Vicat Softening Point 61.7 °C
143 °F
ASTM D1525
ExxonMobil POLYBILT™ PB 152 Bitumen Modifier Resin  (discontinued **)
Polybilt PB 152 is an 18% VA copolymer that yields modified bitumen blends with good storage stability, increased softening point, increased high temperature viscosity and decreased penetration. PB ..