ExxonMobil LLDPE LL 6301RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Exxon Chemical
Trade Name LLDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LLDPE LL 6301RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LL 6301 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Slip: NoThermal Stabilizer: Yes Applications: Cable compound applications LV silane cross-linkable insulation – step processMasterbatch Base ResinInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
ExxonMobil method
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point <= 257 °C
<= 495 °F
Peak Melting Point; ExxonMobil method
Electrical Properties Metric English Comments
Volume Resistivity 7.00e+15 ohm-cm
7.00e+15 ohm-cm
ASTM D257
Dielectric Constant 2.2

@Frequency 60.0 Hz
2.2

@Frequency 60.0 Hz
ASMT D150
Dielectric Strength 59.1 kV/mm
1500 kV/in
500 V/sec; ASTM D149
Dissipation Factor 0.00050

@Frequency 60.0 Hz
0.00050

@Frequency 60.0 Hz
ASMT D150
Users viewing this material also viewed the following: