Ensinger TECACRYL®

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Ensinger
Trade Name TECACRYL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger TECACRYL®.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECACRYL® offers excellent weather resistance, high light transmission, high mechanical strength, high surface hardness and mar resistance, good melt flow rate, and versatile colorability due to crystal clarity. In addition, a special property of TECACRYL polymer includes superior heat resistance and a high level of transparency.Good TransparencyExceptional DurabilityExcellent Mechanical StrengthBecause it is tough, more transparent than glass and twice as light, TECACRYL is ideal for a wide variety of commercial and industrial applications.Information provided by Ensinger
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Water Absorption 0.30 %

@Time 86400 sec
0.30 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 94
94
ASTM D785
Tensile Strength, Yield 65.5 MPa
9500 psi
ASTM D638
Elongation at Yield 4.0 - 6.0 %
4.0 - 6.0 %
ASTM D638
Tensile Modulus 3.24 GPa
470 ksi
1mm/min; ASTM D638
Flexural Strength 117 MPa
17000 psi
ASTM D790
Flexural Modulus 3.38 GPa
490 ksi
ASTM D790
Compressive Strength 117 MPa
17000 psi
ASTM D695
Izod Impact, Notched 0.192 J/cm
0.360 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
long term
Deflection Temperature at 1.8 MPa (264 psi) 93.9 °C
201 °F
ASTM D648
Vicat Softening Point 105 °C
221 °F
ASTM D3418
Flammability Test 300
300
[°F]
Optical Properties Metric English Comments
Haze <= 1.0 %
<= 1.0 %
ASTM D1003
Yellow Index <= 1.0 %
<= 1.0 %
ASTM D1925
Transmission, Visible 92 %
92 %
ASTM D1003