Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Griltech Grilamid® HP 1200 Nylon 12 Fiber (Staple Length = 43)

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer EMS-Griltech
Trade Name Grilamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Griltech Grilamid® HP 1200 Nylon 12 Fiber (Staple Length = 43).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: GRILAMID HP 1200 is a Nylon 12 fiber used in hybrid yarns and as a matrix in composite materials.Data provided by EMS-Griltech.
Physical Properties Metric English Comments
Fiber Count 2.20 dtex
1.98 denier
Descriptive Properties Value Comments
Color Raw White
Luster Bright
Staple Length 43 mm
Users viewing this material also viewed the following: