DuPont Teijin Films Teijin® Tetoron® HB3 Polyester Film, 300 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Teijin® Tetoron®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Teijin® Tetoron® HB3 Polyester Film, 300 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Teijin® Tetoron® HB3 is a super smooth polyester film with a UV absorbing agent, originally designed for green house applications. It has excellent weather-durability, low color and low haze. It is pretreated on one side for slip and is available plain or knurled. Typical Applications: Greenhouse filmOpen air LabelsSolar Window FilmInformation provided by DuPont.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 140 %
140 %
ASTM D882A
Film Elongation at Break, TD 100 %
100 %
ASTM D882A
Coefficient of Friction, Dynamic 0.31
0.31
ASTM D1894
Coefficient of Friction, Static 0.33
0.33
ASTM D1894
Film Tensile Strength at Break, MD 264.93 MPa
38425 psi
ASTM D882A
Film Tensile Strength at Break, TD 283.9 MPa
41180 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 1.0 %

@Temperature 150 °C,
Time 1800 sec
1.0 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 100 °C,
Time 1800 sec
1.0 %

@Temperature 212 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Haze 0.50 %
0.50 %
ASTM D1003
Users viewing this material also viewed the following: