Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 264.93 MPa | 38425 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® G2 Polyester Film, 100 Gauge Teijin® Tetoron® G2 is a polyester film which has high clarity and good slip characteristics.Teijin® Tetoron® G2 is available in the following variations:G2: Non-pretreatedG2N: Adhesion Pretreat.. |
|||
Film Tensile Strength at Break, MD | 264.93 MPa | 38425 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® HB3 Polyester Film, 300 Gauge Teijin® Tetoron® HB3 is a super smooth polyester film with a UV absorbing agent, originally designed for green house applications. It has excellent weather-durability, low color and low haze. It i.. |