Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by DuPont Packaging Polymers.An exceptionally strong polyester film designed to package foods. The film is suitable for heating food products in microwave or conventional ovens. Can be used to package, distribute, and heat foods up to 204°C (400°F).
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Average value for Mylar® films.
Moisture Vapor Transmission 0.600 cc-mm/m²-24hr-atm
1.52 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
Water Vapor Transmission 43.0 g/m²/day
2.77 g/100 in²/day
ASTM E96 Procedure E
Oxygen Transmission 1.80 cc-mm/m²-24hr-atm
4.57 cc-mil/100 in²-24hr-atm
or 140 cc/m²-24hr-atm for the film. ASTM D3985
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 110 %
110 %
ASTM D882
Film Elongation at Break, TD 80 %
80 %
ASTM D882
Modulus of Elasticity 3.79 GPa
550 ksi
(stiffness), ASTM D882
Tear Strength Test 300
300
Graves, g; ASTM D1004
Seal Strength 247 g/25 mm
247 g/in
Film Tensile Strength at Break, MD 186 MPa
27000 psi
ASTM D882
Film Tensile Strength at Break, TD 234 MPa
33900 psi
ASTM D882
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Foods can be heated or cooked up to this temperature.