Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 376 Polyester Film Melinex® 376 is a translucent, smooth, matte polyester film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Information provided by DuPont. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 690 Polyester Film, 142 Gauge Melinex® 690 is a super clear polyester film pretreated on both surfaces to give superior solvent adhesion and improved handleability.Information provided by DuPont. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® 850H Polyester Film, 48 Gauge Mylar® 850H (also called Mylar® 850) is a co-extruded, one side amorphous, heat sealable polyester film designed to be used in metallized, print, and lamination applications. This film is suitable.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® 854 Polyester Packaging Film, 60 Gauge Data provided by DuPont Packaging Polymers.DuPont Melinex® DuPont Melinex® 854 is a clear, one side coextruded heat sealable surface similar to Melinex® 850. The opposite surface is adhesion pret.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® CL Polyester Film, 50 Gauge Mylar® CL is an exceptionally strong polyester film designed to package foods. Foods can be heated or cooked in this film at temperatures up to 400°F. Mylar® CL is commercially available in nomin.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EC Polyester Film, 200 Gauge Mylar® EC films are electrical grade films designed for use in applications where improved dimensional stability is required. In addition to lower levels of shrinkage, Mylar® EC films offer outsta.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EL Polyester Film, 300 Gauge Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EL Polyester Film, 500 Gauge Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EL21 Polyester Film, 1000 Gauge Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EL21 Polyester Film, 750 Gauge Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882 |
DuPont Teijin Films Mylar® LB Polyester Film, 48 Gauge (12 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester film designed for use as a component of a lamination. Standard thickness offered include 48, 75, and 92 gauges. Variet.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882 |
DuPont Teijin Films Mylar® LBT Polyester Film, 48 Gauge (12 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester film that has been corona-treated to provide superior wetting and adhesion to inks, primers, and adhesives. Standard th.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® LBTW Polyester Film, 92 Gauge Mylar® LBTW is an uncoated, transparent polyester film that has been corona treated on one side to provide superior wetting and adhesion of inks, primers, and adhesives. Mylar® LBTW is commerciall.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MDA Polyester Film, 1000 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MDA Polyester Film, 750 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MO21 Polyester Film, 1000 Gauge Product Description: Mylar® type MO21 films are strong, heavy gauge films that have excellent electrical properties. These films offer exceptional cut-through resistance, low shrinkage, low moistur.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MO21 Polyester Film, 900 Gauge Product Description: Mylar® type MO21 films are strong, heavy gauge films that have excellent electrical properties. These films offer exceptional cut-through resistance, low shrinkage, low moistur.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® OWF Polyester Film, 80 Gauge Product Description: Mylar® OWF is a co-extruded, one side amorphous, heat sealable polyester film designed to be used as an overwrap film. This film is suitable for use in contact with food. Appro.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® WC11/WC22 Polyester Film, 300 Gauge Mylar® type WC11 films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectric and good handlin.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 535 Polyester Film Melinex® 535 is a high clarity polyester film that is two-side pretreated to promote adhesion to aqueous based coatings.Information provided by DuPont. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 623 Polyester Film, 500 Gauge Melinex® 623 is a super clear polyester film pretreated on both surfaces to give superior solvent adhesion and improved handleability.Information provided by DuPont. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882 |
DuPont Teijin Films Mylar® 50 OL Polyester Film, Ovenable Lidding, Heat Sealable, 50 Gauge Data provided by DuPont Packaging Polymers.An exceptionally strong polyester film designed to package foods. The film is suitable for heating food products in microwave or conventional ovens. Can b.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® 850H Polyester Film, 80 Gauge Mylar® 850H (also called Mylar® 850) is a co-extruded, one side amorphous, heat sealable polyester film designed to be used in metallized, print, and lamination applications. This film is suitable.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® A Polyester Film, 300 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® A Polyester Film, 500 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® A Polyester Film, 750 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EL21 Polyester Film, 900 Gauge Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MDA Polyester Film, 300 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MDA Polyester Film, 900 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Film Tensile Strength at Break, MD | 186 MPa | 27000 psi | ASTM D882 |
DuPont Teijin Films Mylar® M30 Polyester Film, 50 Gauge (14 µm), PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and.. |