Material Notes:
Melinex® 376 is a translucent, smooth, matte polyester film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 100 MPa
14500 psi
ASTM D882A
Film Tensile Strength at Yield, TD 103 MPa
15000 psi
ASTM D882A
Film Elongation at Break, MD 115 %
115 %
ASTM D882A
Film Elongation at Break, TD 80 %
80 %
ASTM D882A
Coefficient of Friction, Dynamic 0.30
0.30
ASTM D1894
Film Tensile Strength at Break, MD 186 MPa
27000 psi
ASTM D882A
Film Tensile Strength at Break, TD 214 MPa
31000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.8 %

@Temperature 190 °C,
Time 300 sec
2.8 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 0.00 %

@Temperature 190 °C,
Time 300 sec
0.00 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Gloss 28 %
28 %
45°; ASTM D1003
38 %
38 %
60°; ASTM D1003
Transmission, Visible 80 %

@Thickness 0.0234 mm
80 %

@Thickness 0.000920 in
TLT; ASTM D1003
85 %

@Thickness 0.0191 mm
85 %

@Thickness 0.000750 in
TLT; ASTM D1003