Dow VORANOL™ CP 4702 Polyol

Category Polymer , Thermoset
Manufacturer Dow Chemical
Trade Name VORANOL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow VORANOL™ CP 4702 Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
VORANOL™ CP 4702 polyol is a high reactivity, capped triol, polyether polyol especially designed for the production of molded flexible foam. It is normally used in all TDI or TDI/MDI blend formulations.Information provided by Dow
Physical Properties Metric English Comments
Specific Gravity 1.026 g/cc
1.026 g/cc
pH 7.0 - 9.0
7.0 - 9.0
(1 Water / 10 Methanol); DOWM 101495-TE94A
Viscosity Measure 434 cSt

@Temperature 37.8 °C
434 cSt

@Temperature 100 °F
ASTM D445-94
750 - 870 cSt

@Temperature 25.0 °C
750 - 870 cSt

@Temperature 77.0 °F
ASTM D445-94
Molecular Weight 4700 g/mol
4700 g/mol
Maximum Moisture Content 0.060
0.060
wt% water; ASTM E203-96
ASTM Color <= 30
<= 30
APHA; ASTM D4890-93
Thermal Properties Metric English Comments
Flash Point 248 °C
478 °F
C.O.C.
Chemical Properties Metric English Comments
Total Acid Number 0.050
0.050
[mg KOH/g]; DOWM 100387-TE95A
Descriptive Properties Value Comments
Hydroxyl Number mg KOH/g 33.7 - 37.3
ASTM D4274-94d